Steel Wire Rope Of 12 Mm Diameter Fiber Main Core Ungalvanised, Roh Lay 6X37 Constructio N, Tensile Designation 1770 N/Mm2, Minimum Breaking Load 75 Kn As Per Is 2266:2019 Or Latest. Make: Us Ha Martin / Mahadev / Bharat Wire Rope / Asahi / Well Worth Only. Firm Must Submit Load Test Certificate Iss Ued By Nabl Approved Lab / Govt. Approved/ Govt. Test House Along With Supply. [ Warranty Period: 12 Months After The Date Of Delivery ] ]